Surface preparation & application

  1. Clean the surface to be painted by removing all loose particles, grease, dirt, rust etc.
  2. Stir contents thoroughly.
  3. Apply Indigo Zinc Chromate Primer using brush or spray after thinning 15-20% with turpentine. Allow the film to dry overnight before applying the topcoat.

How long does it take for zinc chromate to dry?

DRYING & CURING SCHEDULE Primer dries dust free in 5 minutes and dries hard in 15 minutes. Times may vary depending on climate, temperature, and atmospheric conditions.

How does zinc chromate primer protect a surface?

This compound was a useful coating because it is an anti-corrosive and anti-rust primer. Since it is highly toxic, it also destroys organic growth on the surface. Zinc chromate is also used in spray paints, artists’ paints, pigments in varnishes, and in making linoleum.

What is the difference between zinc chromate vs zinc phosphate primer?

In general, zinc chromate is a more effective and robust than zinc phosphate. Zinc chromate is epoxy based, while zinc phosphate is an alkyd, which means zinc chromate is more durable when used in a primer. Studies have found that zinc chromate is harmful and carcinogenic to humans.

What does zinc chromate primer do?

Zinc chromate is used for a wide range of applications. It is an odorless chemical compound primarily used as an industrial paint coating. The compound is a beneficial coating because it is an anti-corrosive and an anti-rust primer. It is primarily used to coat aluminum and iron materials.

Can you paint over yellow zinc?

A. Generally you can use the same paints on zinc plating as you do when you paint over galvanizing. I strongly suggest that you first pretreat the surface with either an iron or zinc phosphate process. Select the appropriate coating system based on the type of exposure to which the painted product will be exposed.

What is the purpose of zinc primer?

Zinc-rich primers offer excellent adhesion properties, as well as galvanic protection for structural steel surfaces. When in contact with structural steel, zinc primers corrode preferentially to the steel, protecting it from damage.

Which paint is best for zinc?

Galvanized paint is a popular zinc-based paint that protects metal surfaces from rust and corrosion. Both cold galvanizing paint and hot-dip galvanizing paint can be used, but the latter is the preferred choice for professionals.

Does paint stick to zinc plating?

A. Generally you can use the same paints on zinc plating as you do when you paint over galvanizing. I strongly suggest that you first pretreat the surface with either an iron or zinc phosphate process.

How long does it take pt-522 zinc chromate primer to dry?

Primer dries dust free in 5 minutes and dries hard in 15 minutes. Times may vary depending on climate, temperature, and atmospheric conditions.Always bring the coating to the “tack free” stage before top coating.

Can you use zinc chromate as a primer?

Yes, it can be done in your garage. Since it is primer, I just shoot it outside. If you’re looking for something easy to squirt that offers good (not maximum) corrosion protection and “OK’ paint adhesion, try zinc chromate in a spray can.

What kind of primer do you use for PTI paint?

PT-522 Zinc Chromate Primer — TT-P-1757 TYI CLASS C & N is a general purpose, rust inhibitive, alkyd primer. It is intended for use over metals that are bare, scuffed, sanded, lightly rusted, abrasive blast and previously painted surfaces while showing excellent anti-corrosion properties.

What are the side effects of zinc chromate exposure?

* Zinc Chromatecan irritate the skin causing a rash or skin ulcers. * Exposure to Zinc Chromatecan irritate the eyes, nose, and throat. * Repeated exposure can cause sores in the nose and/or a hole in the bone dividing the inner nose (septum), sometimes with bleeding, discharge or crusting. *Zinc Chromatemay cause a skin allergy.