Alloy 347 (S34700) is stabilized stainless steel plate which offers as its main advantage an excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800 to 1500°F (427 to 816°C).

What is SS316 material?

Stainless steel 316 (SS316) is an austenitic chromium-nickel stainless steel containing deliberate amount of molybdenum which increases general corrosion resistance and especially improves its pitting resistance to chloride ion solutions.

What is 347 stainless steel used for?

Alloy 347/347H In the food and beverage manufacturing and processing industry, it is common for stainless steel to be used for everything from containers, vats, ovens and piping systems to bulk storage tanks, machinery parts, valves, fittings and other food contact equipment.

What is SS 316 grade?

What is 316 Stainless Steel? Grade 316 is a popular alloy of stainless steel with a melting range of 2,500 °F – 2,550 °F (1,371 °C – 1,399 °C). As an austenitic stainless steel alloy, it has qualities such as high strength, corrosion resistance, and high concentrations of chromium and nickel.

Which is better alloy 347h or s3409?

The alloy has good oxidation resistance and creep strength to 1500°F (816°C). It also possesses good low temperature toughness. Alloy 347H (UNS S3409) is the higher carbon (0.04 – 0.10) version of the alloy. It was developed for enhanced creep resistance and for higher strength at temperatures above 1000°F (537°C).

Which is higher carbon 347 or 347h stainless steel?

Alloy 347H (UNS S3409) stainless steel plate is the higher carbon (0.04 – 0.10) version of the alloy. It was developed for enhanced creep resistance and for higher strength at temperatures above 1000°F (537°C).

Can a Grade 347h stainless steel be annealed?

The grade 347H steel has to be water quenched and annealed to obtain maximum hardness. Grade 347H stainless steel can be readily stamped, blanked, spun and drawn as it is quite tough and ductile. Grade 347H stainless steel can be annealed at temperature ranging from 1010 to 1193°C (1850 to 2000°F) and then quenched with water.